Analysis on the causes of longitudinal thin and thick of plastic wire drawing extrusion film
添加時間:2024-08-31
 

Resin plasticizing bad, may be inappropriate given: the heating zone temperature control instrument malfunction, resin mixed with different melt index and density of other relevant major resin: extruder factors such as low back pressure. Under the microscope (40 times), there is no melting point. The extrusion film is dark, opaque and viscous. The most effective way to determine malplasticization is to check under a microscope for non-molten materials.

In the case of fault treatment, the first method to eliminate the mixing of other resins in the resin is to measure the melting index, which is determined after comparing with the standard index. Then consider adjusting the temperature of each heating area to check the temperature controller. If the temperature controller in the heating zone is found to be heated all the time without reaching the given temperature, the screw speed can be reduced to achieve good plasticization. Increasing the back pressure of the extruder can increase the number of filter mesh, but too high back pressure will damage the screw thrust bearing of the extruder. For the failure of on-site temperature control, raw material and flow rate to achieve stable melt film and low production capacity, it is necessary to consider changing screw design and replacing high-efficiency screw.


?
推薦產品 Recommended Products
聯系我們 contact us
0576- 85863788
手機:
13819698788
傳真:
0576-85323785
郵箱:
dhj0905@163.com
地址:
浙江臨海市古城街道兩水工業區義城路71號
? 主站蜘蛛池模板: 平定县| 依安县| 龙泉市| 榆中县| 察隅县| 绥江县| 蓬溪县| 南宁市| 木里| 普洱| 新安县| 南靖县| 乐亭县| 永年县| 墨脱县| 麻阳| 碌曲县| 家居| 宝清县| 鄂伦春自治旗| 花垣县| 杭锦旗| 娱乐| 乐东| 蚌埠市| 咸丰县| 白山市| 礼泉县| 阳泉市| 手机| 阿勒泰市| 鄂州市| 连云港市| 乌拉特中旗| 勃利县| 军事| 济南市| 金乡县| 阳朔县| 和政县| 阿拉善左旗|